模塑收缩量, flow, 0.125" | ASTM D-955 | 5-7 | in/in E-3 | |
模塑收缩量, xflow, 0.125" | ASTM D-955 | 5-7 | in/in E-3 | |
密度, 固体 | ASTM D-792 | 1.11 |
仪表控制抗冲击能量 @ 峰值, -22F. | ASTM D-3763 | 8.6 | ft-lbs | |
拉伸伸长, 断裂, 类型 I 0.125" | ASTM D-638 | 17.0 | % | |
伊佐德冲击值, 反向缺口, -22F | ASTM D-256 | 12.0 | ft-lb/in | |
抗拉强度, 屈服, 类型 I, 0.125" | ASTM D-638 | 9700 | psi | |
伊佐德冲击值, 缺口, 73F | ASTM D-256 | 3.5 | ft-lb/in | |
挠曲强度, 屈服, 0.250 | ASTM D-790 | 14400 | psi | |
伊佐德冲击值, 缺口, -22F | ASTM D-256 | 1.8 | ft-lb/in | |
挠曲模量, 0.250" | ASTM D-790 | 361500 | psi | |
拉伸伸长, 屈服, 类型 I 0.125" | ASTM D-638 | 8.0 | % | |
伊佐德冲击值, 反向缺口, 73F | ASTM D 256 | 16.6 | ft-lb/in | |
仪表控制抗冲击能量 @ 峰值, 73F. | ASTM D-3763 | 29.0 | ft-lbs | |
抗拉强度, 断裂, 类型 I, 0.125" | ASTM D 638 | 7200 | psi |
HDT(热畸变温度), 66 psi, 0.250", 未退火 | ASTM D-648 | 229 | deg F | |
UL文件号, 美国 | E121562 | |||
V-0 额定值 | 测试厚度 | UL 94 | 0.060 | inch |
HDT(热畸变温度), 264 psi, 0.250",未退火 | ASTM D-648 | 211 | deg F | |
维卡软化温度, B级 | ASTM D-1525 | 264 | deg F | |
热指数, 机械冲击性能 | UL 746B | 80 | deg C | |
热指数, 非机械冲击性能 | UL 746B | 95 | deg C | |
热指数, 电性能 | UL 746B | 95 | deg C | |
5VA 额定值 | 测试厚度 | UL 94 | 0.120 | inch |
损耗因数, 50 Hz | ASTM D-150 | 0.0100 | ||
表面电阻率 | ASTM D-257 | >1 E14 | ohm/sq | |
体积电阻率 | ASTM D-257 | 2E+16 | ohm-cm | |
介电常数, 50 Hz | ASTM D-150 | 2.69 | ||
损耗因数, 1 MHz | ASTM D-150 | 0.0070 | ||
介电强度, 油内, 125 mils | ASTM D-149 | 414 | v/mil | |
介电常数, 1 MHz | ASTM D-150 | 2.55 |